Input-output norms require specified input proportions for cast alloy permanent magnet exports and matching imports to export use. Standard Input-Output Norms set material consumption ratios for cast alloy permanent magnet exports: cobalt and nickel 1.05 kg/kg export, pure iron 1.20 ... Summary
Input-output norms require specified input proportions for cast alloy permanent magnet exports and matching imports to export use.
Standard Input-Output Norms set material consumption ratios for cast alloy permanent magnet exports: cobalt and nickel 1.05 kg/kg export, pure iron 1.20 kg/kg, aluminium ingot 1.10 kg/kg, and copper 1.10 kg/kg. Applicants must ensure imported inputs correspond to and are actually used in the manufacture of the export product; proportions are subject to determination and verification against these norms.
Full Summary is available for active users!